Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 425 MPa
>= 61600 psi
MetalTek MTEK 20 Cast UNS N08007 Super Austenitic Stainless Steel
Corrosion resistance approaching nickel alloys, especially in chloride service.Applications: Process piping exposed to flue gas and solutions.Information provided by MetalTekCast UNS N08007; Cast Gr..
Tensile Strength, Ultimate 425 MPa

@Temperature 870 °C
61600 psi

@Temperature 1600 °F
Haynes 25 alloy, cold worked sheet, 10% cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate <= 425 MPa
<= 61600 psi
CLAL-MSX NICLAL 1300 0 Annealed Copper Alloy, Free Cutting Nickel-Silver
Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX