Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 42.1 MPa | 6110 psi | ASTM D638 |
Plaskolite Optix® CA-1000 I Clear High Impact Acrylic Resin High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resi.. |
|||
Tensile Strength, Ultimate | 42.1 MPa | 6110 psi | ASTM D638 |
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resi.. |