Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 4.20 MPa | 609 psi | ASTM D638 |
ExxonMobil Escorene® UL-7740 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Tensile Strength, Ultimate | 4.20 MPa @Temperature 49.0 °C |
609 psi @Temperature 120 °F |
Type IV, crosshead speed 2 in/min; ASTM D638 |
DuPont Elvax® 265 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |