Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6000 MPa | 870000 psi | Virgin Filament |
Saint-Gobain Quartzel® Fused Quartz Textiles Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava.. |
|||
Tensile Strength, Ultimate | 6000 MPa | 870000 psi | |
Hexcel® IM9 Carbon Fiber (12,000 Filaments) Weight/length = 0.331 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |