Polymer Property : Tensile Strength, Ultimate = 60.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.5 MPa
8770 psi
ASTM D638
Plenco 4100 Phenolic, Granular, Compression Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and ..
Tensile Strength, Ultimate 60.5 MPa
8770 psi
ASTM D638
Plenco 4759 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and possesses good electrical properties. It is used in appli..