Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.70 MPa | 972 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 8109 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 6.70 MPa | 972 psi | TPE-0153 (ASTM D 412) |
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer designed for glazing and sealing applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonat.. |
|||
Tensile Strength, Ultimate | 6.70 MPa | 972 psi | |
Freudenberg Simrit SC1217 S317 Silicone Elastomer Excellent material for static service at extreme (hot or cold) temperatures. Outstanding flex and fatigue life. Very good for ozone and UV radiation service as well as for resistance to fungal and b.. |