Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 6.55 MPa
950 psi
Original Properties; ASTM D412 Die C
Freudenberg Simrit S50 Silicone Elastomer (VMQ)
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol..
Tensile Strength, Ultimate 6.55 MPa
950 psi
Original Properties; ASTM D412 Die C
Freudenberg Simrit S60 Silicone Elastomer (VMQ)
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol..
Tensile Strength, Ultimate 6.55 MPa
950 psi
Sylvin Technologies 8999-60 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 6.55 MPa
950 psi
Sylvin Technologies 9999-60 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 6.55 MPa
950 psi
Colorite Polymers Flexchem 4051-02 Vinyl Compound
Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds ut..
Tensile Strength, Ultimate 6.55 MPa
950 psi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 6.55 MPa
950 psi
ASTM D638
Colorite Polymers 4543 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 6.55 MPa
950 psi
ASTM D412
Arlon R3792-920-10R##-P0 Silicone Rubber
This self-fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicon..