Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.44 MPa | 934 psi | post cured- 2 hours at 200°C; ASTM D412 |
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |