Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.0420 MPa | 6.09 psi | |
Zircar Refractory Composites RSBL-SOL8 Silica-Magnesia Blanket ZIRCAR Refractory Composites, Inc. insulating blankets are non woven, inorganic, fiber-based products that contain no asbestos. They are engineered for use as thermal barrier materials in high tempe.. |