Polymer Property : Tensile Strength, Ultimate = 591 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 591 MPa
85700 psi
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 16.4% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..