Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4.00 MPa
580 psi
ASTM D412
Multibase Multi-Flex® TPE A 8299 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 4.00 MPa
580 psi
ASTM D412
Multibase Multi-Flex® TPE RP 6568 CT BLK
Ash is 1.35%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 4.00 MPa
580 psi
Pyrotek Pyroboard™ S1100 Roller
Pyroboard™ S1100 is an economical material that is perfect for one time use on new campaigns.Information provided by Pyrotek.
Tensile Strength, Ultimate 4.00 MPa
580 psi
ambient temperature
Pyrotek U-1 Compressible Board
U-1 is a high-temperature millboard that is easily cut, punched and shaped. It works well as a roll-cladding material and as compressible gasketing. A unique characteristic of the asbestos-free bo..
Tensile Strength, Ultimate 4.00 - 137 MPa
580 - 19900 psi
Average value: 70.9 MPa Grade Count:73
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Tensile Strength, Ultimate >= 4.00 MPa
>= 580 psi
ASTM D412
Multibase Multi-Flex® TPE A 4410 NAT
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate >= 4.00 MPa
>= 580 psi
ASTM D412
Multibase Multi-Flex® TPE A 6221 C BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate >= 4.00 MPa
>= 580 psi
ASTM D412
Multibase Multi-Flex® TPE A 6221 C NAT
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate >= 4.00 MPa
>= 580 psi
ASTM D412
Multibase Multi-Flex® TPE A 6221 E UV BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate 4.00 - 35.0 MPa
580 - 5080 psi
ASTM D638
Dow Engage® Polyolefin Elastomer
Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. ..
Tensile Strength, Ultimate 4.00 - 9.00 MPa
580 - 1310 psi
ATG s.r.l. VMQ Silicone Rubber