Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 58.2 MPa | 8440 psi | ASTM D638 |
Nylene® Naxel™ PC530-112 UV Resistant Polycarbonate Description: Naxel™ PC530-112 is a high flow, UV resistant polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resour.. |