Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 440 - 560 MPa | 63800 - 81200 psi | |
Materion Beryllium Copper Alloy 10 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 440 - 560 MPa | 63800 - 81200 psi | |
Materion Beryllium Copper Alloy 10 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 440 - 560 MPa | 63800 - 81200 psi | |
Materion Beryllium Copper Alloy 3 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 490 - 560 MPa | 71100 - 81200 psi | |
SSAB Tunnplat Aluzink 420A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Tensile Strength, Ultimate | 490 - 560 MPa | 71100 - 81200 psi | |
SSAB Tunnplat Dogal 420YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Tensile Strength, Ultimate | 460 - 560 MPa | 66700 - 81200 psi | |
CLAL-MSX NICLAFOR® 1000 TD1 Quenched/Cold Rolled, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Tensile Strength, Ultimate | 520 - 560 MPa | 75400 - 81200 psi | L direction |
ArcelorMittal Save 20-13 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Ultimate | 520 - 560 MPa | 75400 - 81200 psi | L direction |
ArcelorMittal Save 25-14 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Ultimate | 520 - 560 MPa | 75400 - 81200 psi | L direction |
ArcelorMittal Save 27-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Ultimate | 520 - 560 MPa | 75400 - 81200 psi | L direction |
ArcelorMittal Save 30-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Ultimate | 440 - 560 MPa | 63800 - 81200 psi | |
Materion Beryllium Copper Alloy 3 Tube; H (TD04) Temper; up to 76 mm o.d. (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 440 - 560 MPa | 63800 - 81200 psi | |
Materion Beryllium Copper Alloy 3 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |