Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 558 - 607 MPa | 81000 - 88000 psi | Average value: 578 MPa Grade Count:5 |
Overview of materials for Nylon 6 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Tensile Strength, Ultimate | 558 MPa | 80900 psi | Longitudinal Orientation, True Stress/True Strain |
AK Steel 13-4 SR® Ferritic Stainless Steel AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w.. |
|||
Tensile Strength, Ultimate | 558 MPa | 80900 psi | |
AK Steel 316L Austenitic Stainless steel AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.Information provided by AK Steel |