Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 546 MPa | 79200 psi | |
ATI Wah Chang TI-45 Nb Applications: Aerospace Rivet Material; High Pressure Oxygenated Gas Vents; Superconducting Wire Information provided by ATI Wah Chang |
|||
Tensile Strength, Ultimate | 546 MPa | 79200 psi | 10% Cold Worked |
AK Steel 439 ULTRA FORM® Stainless Steel AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul.. |