Polymer Property : Tensile Strength, Ultimate = 54400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 375 MPa

@Temperature 300 °C
54400 psi

@Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..
Tensile Strength, Ultimate 375 MPa

@Temperature 400 °C
54400 psi

@Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..
Tensile Strength, Ultimate 375 MPa

@Temperature 300 °C
54400 psi

@Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Tensile Strength, Ultimate 375 MPa

@Temperature 400 °C
54400 psi

@Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Tensile Strength, Ultimate 375 MPa

@Temperature 649 °C
54400 psi

@Temperature 1200 °F
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel
Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated..
Tensile Strength, Ultimate 375 MPa

@Temperature 300 °C
54400 psi

@Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..
Tensile Strength, Ultimate 375 MPa

@Temperature 400 °C
54400 psi

@Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..