Polymer Property : Tensile Strength, Ultimate = 541000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3730 MPa
541000 psi
Hexcel® UHM Carbon Fiber (12,000 Filaments)
Weight/length = 0.341 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Tensile Strength, Ultimate 3730 MPa
541000 psi
Hexcel® UHM Carbon Fiber (3000 Filaments)
Weight/length = 0.085 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..