Polymer Property : Tensile Strength, Ultimate = 54100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 373 MPa

@Temperature 371 °C
54100 psi

@Temperature 700 °F
AK Steel 439 ULTRA FORM® Stainless Steel
AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul..