Polymer Property : Tensile Strength, Ultimate = 53000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 365 - 427 MPa
53000 - 62000 psi
Eagle Brass 151 ZHC® COPPER, Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Tensile Strength, Ultimate 365 - 434 MPa
53000 - 63000 psi
Eagle Brass 194 HSM® Copper, 1/2 Hard
High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl..
Tensile Strength, Ultimate 365 - 455 MPa
53000 - 66000 psi
Eagle Brass 519 Phosphor Bronzes 6%, 1/4 Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
Tensile Strength, Ultimate 365 - 434 MPa
53000 - 63000 psi
Eagle Brass 752 Nickel Silver 18%, Annealed
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info..
Tensile Strength, Ultimate 365 MPa
53000 psi
annealed
CMW® ELKONIUM 22 silver, copper alloy
Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a..