Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 35.8527 - 35.8527 MPa

@Temperature 149 - 149 °C
5200.01 - 5200.01 psi

@Temperature 300 - 300 °F
Average value: 35.9 MPa Grade Count:1
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..