Polymer Property : Tensile Strength, Ultimate = 52.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 52.3 MPa
7590 psi
ASTM Data
Styron Pulse® B250 ABS + Polycarbonate
PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. ..