Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 517.1 MPa | >= 75000 psi | |
ATI Allegheny Ludlum Type 310L Stainless Steel Corrosive attack of stainless steels by concentrated nitric acid often results in preferential attack of grain boundaries. The high Cr content combined with restricted levels of C, Si, P, S, and Mo .. |