Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 515 MPa | 74700 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4724 High Temperature Ferritic Stainless Steel Truly stainless high temperature grade with 13% chromium. Not critical in terms of embrittlement.Applications: Mostly used in high temperature applications with sulphurous atmospheres and/or low te.. |
|||
Tensile Strength, Ultimate | >= 515 MPa | >= 74700 psi | |
MetalTek MTEK 175 Cast UNS C95400 Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Ultimate | >= 515 MPa | >= 74700 psi | |
MetalTek MTEK 317L Cast UNS J92999 Austenitic Stainless Steel "300" series, general corrosion resistant alloyApplications: Nuclear, chemical and food processing. Valve and pump trim.Information provided by MetalTek |
|||
Tensile Strength, Ultimate | >= 515 MPa | >= 74700 psi | |
MetalTek MTEK 275 Cast UNS C95900 Aluminum Bronze Engineered alloy for excellent wear and anti-galling properties in forming, bending and drawing dies. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information provide.. |
|||
Tensile Strength, Ultimate | >= 515 MPa | >= 74700 psi | |
MetalTek MTEK 27-5 Cast UNS J93015 Heat Resistant Stainless Steel Higher nickel yields improved strength. Resists high sulfur process gas.Applications: Pour spouts, holding pots, kiln parts, gas parts.Information provided by MetalTek |
|||
Tensile Strength, Ultimate | >= 515 MPa | >= 74700 psi | |
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Tensile Strength, Ultimate | >= 515 MPa | >= 74700 psi | |
ATI Allegheny Ludlum Stainless Steel Type 348 (UNS S34800) AL 348 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |
|||
Tensile Strength, Ultimate | >= 515 MPa | >= 74700 psi | Annealed; Min required by ASTM A 240 and ASME SA-240 |
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Tensile Strength, Ultimate | >= 515 MPa | >= 74700 psi | |
ATI Allegheny Ludlum Stainless Steel Type 347 (UNS S34700) AL 347 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |