Polymer Property : Tensile Strength, Ultimate = 50900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 351 MPa

@Temperature 593 °C
50900 psi

@Temperature 1100 °F
AK Steel 441 Ferritic Stainless steel
AK Steel 441 is a 17-18% by weight, chromium and columbium bearing ferritic stainless steel which provides good high-temperature strength (exceeding that of Types 409 and AK Steel 439 LT Stainless S..