Tensile Strength, Ultimate 3.50 MPa
508 psi
ASTM D412
Multibase Multi-Flex® TPE A 7020 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 3.50 MPa

@Temperature 800 °C
508 psi

@Temperature 1470 °F
Pyrotek U-1 Compressible Board
U-1 is a high-temperature millboard that is easily cut, punched and shaped. It works well as a roll-cladding material and as compressible gasketing. A unique characteristic of the asbestos-free bo..