Tensile Strength, Ultimate 5.34 MPa
775 psi
Dow Corning SILASTIC® 25784-V SILICONE RUBBER RED
40 Durometer, peroxide cured, high temperature resistance Silicone Rubber CompoundInformation provided by Dow Corning