Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.1 MPa | 4950 psi | after optimum cure |
Armstrong A-31 Epoxy Adhesive Is a neutral-colored thixotropic paste material having a creamy or buttery consistency that will not flow even when cured at elevated temperatures A-31 also features Extremely low outgassing charact.. |