Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 494 MPa | 71600 psi | Longitudinal to Sheet Rolling Direction, Tensile Hardness Test (ASTM E8, E694, E18, A370) |
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |
|||
Tensile Strength, Ultimate | 494 MPa | 71600 psi | Transverse to Sheet Rolling Direction, Tensile Hardness Test (ASTM E8, E694, E18, A370) |
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |