Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 12.5 - 33.1 MPa | 1810 - 4800 psi | Average value: 22.8 MPa Grade Count:5 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 23.4 - 33.1 MPa | 3390 - 4800 psi | Average value: 28.3 MPa Grade Count:13 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |