Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 470 MPa

@Temperature 400 °C
68200 psi

@Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel
Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr..
Tensile Strength, Ultimate 470 MPa

@Temperature 100 °C
68200 psi

@Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Ultimate 470 MPa

@Temperature 100 °C
68200 psi

@Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Ultimate 470 MPa

@Temperature 100 °C
68200 psi

@Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Tensile Strength, Ultimate 470 MPa

@Temperature 760 °C
68200 psi

@Temperature 1400 °F
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Ultimate 470 MPa

@Temperature 760 °C
68200 psi

@Temperature 1400 °F
Haynes 556® alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Ultimate 470 MPa

@Temperature 300 °C
68200 psi

@Temperature 572 °F
Annealed prior to test
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy
Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a..
Tensile Strength, Ultimate 470 - 570 MPa
68200 - 82700 psi
CLAL-MSX NICLAL 1300 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver
Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX
Tensile Strength, Ultimate 470 MPa
68200 psi
ATI Allegheny Ludlum AL 453™ Stainless Steel
Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum
Tensile Strength, Ultimate 470 - 590 MPa
68200 - 85600 psi
ArcelorMittal HSLA 420 High strength low alloy steel for cold forming, Cold Rolled
Available in the following: uncoated (HC420LA), electroglavanized (HC420LA +ZE) and Extragal®/galfan/Galvannealed (HC420LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range ..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 20-15 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 25-16 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 27-16 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 30-17 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Ultimate 470 - 510 MPa
68200 - 74000 psi
L direction
ArcelorMittal Torque 30-18 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..