Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 46.5 MPa | 6750 psi | ASTM D412 |
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos.. |
|||
Tensile Strength, Ultimate | 46.5 MPa | 6750 psi | ASTM D638 |
Colorite Polymers 2018 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |