Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 453 MPa

@Temperature 760 °C
65700 psi

@Temperature 1400 °F
at 760°C after aging
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 760°C (1400°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..