Polymer Property : Tensile Strength, Ultimate = 45.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.310 MPa
45.0 psi
ASTM D412
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam
Medium grade silicon sponge. UL recognized for flame retardance and gasketing.Applications: HID (High Intensity Discharge) lighting fixture gaskets, Battery cushion in hand-held electronic products..
Tensile Strength, Ultimate 0.310 MPa
45.0 psi
ASTM D638
Covestro Bayfill® EA 4002 Polyurethane Energy-Absorbing Semi-Rigid Foam, Rigid Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.