Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 30.6 MPa | 4440 psi | 150°C, 40 min., Pressure Vulcanization. -13% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 25SH Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |