Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 443 MPa @Temperature 316 °C |
64300 psi @Temperature 601 °F |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |