Polymer Property : Tensile Strength, Ultimate = 410 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.83 MPa
410 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9111-35W222 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for use in difficult injection molding applications and those requiring good flex..
Tensile Strength, Ultimate 2.83 - 14.0 MPa
410 - 2030 psi
Average value: 10.7 MPa Grade Count:15
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an..