Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 41.7 MPa | 6050 psi | after optimum cure |
Armstrong A-40 Epoxy Adhesive Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re.. |
|||
Tensile Strength, Ultimate | 41.7 MPa | 6050 psi | cured 2 hours @ 93°C |
Abatron AboCast 8110-9/AboCure 50-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Tensile Strength, Ultimate | 41.7 MPa | 6040 psi | ASTM D638 |
Samyang Triel® 5720 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5720 is an extrusion grade.Information provided by Samyang. |
|||
Tensile Strength, Ultimate | 41.7 MPa | 6040 psi | ASTM D638 |
Samyang Triel® 5722EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5722EM is an extrusion grade.Information provided by Samyang. |