Tensile Strength, Ultimate 0.0552 - 2.80 MPa
8.00 - 406 psi
Average value: 0.387 MPa Grade Count:15
Overview of materials for Silicone Foam
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW..