Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 4.69 MPa | 680 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Tensile Strength, Ultimate | 4.69 MPa | 680 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Strength, Ultimate | 4.69 MPa | 680 psi | Across Flow; ASTM D412 |
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |