Polymer Property : Tensile Strength, Ultimate = 4.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4.10 MPa
595 psi
TPE-0153 (ASTM D 412)
ExxonMobil Vyram™ 9271-65 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure..
Tensile Strength, Ultimate 4.10 MPa
595 psi
at max load; ASTM D638
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low ..
Tensile Strength, Ultimate 4.10 MPa
595 psi
at max load; ASTM D638
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low ..
Tensile Strength, Ultimate 4.10 MPa
595 psi
at max load; ASTM D638
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low ..
Tensile Strength, Ultimate 4.10 MPa
595 psi
at max load; ASTM D638
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low ..
Tensile Strength, Ultimate 4.10 MPa
595 psi
at max load; ASTM D638
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low ..
Tensile Strength, Ultimate 4.10 MPa
595 psi
at max load; ASTM D638
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low ..
Tensile Strength, Ultimate 4.10 MPa
595 psi
GB/T 528
Chengdu Polyster 5502 High Performance Grade TPV
Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd.