Polymer Property : Tensile Strength, Ultimate = 39.98 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.98 MPa
5798 psi
ASTM D1708
DSM Biomedical CarboSil® 20 90A Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU)
A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes Th..