Polymer Property : Tensile Strength, Ultimate = 39.24 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.24 MPa
5692 psi
ASTM D1708
DSM Biomedical PurSil® 10 Thermoplastic Silicone Polyether Urethane  (discontinued **)
PurSil® thermoplastic siliconepolyether-urethane (TSPU) is a novel copolymer that is strong, yet flexible with proven biocompatibility and biostability. Leveraging the benefits of both silicone ela..