Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.66 MPa | 386 psi | |
Valley Adhesives EM-222 Low Temperature Application Glue Stick Valley Adhesives EM-222 Low Temperature Application Glue StickRapid strength build up; Excellent hot tacking and wetting; Safe on styrofoam and heat sensitive materials; Bonds corrugated boxes and p.. |