Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2590 MPa
376000 psi
Honeywell Spectra® 900 Fiber
Spectra® fiber 900 was the first commercially available extended-chain, high-strength polyethylene fiber and the first in a series of Spectra® fibers. Spectra® fiber has one of the highest ..