Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.56 MPa | 371 psi | ASTM D 638 |
REXtac Rextac® RT 2180 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point, short open time, good cohesive strength, and high viscosityApplications: Component of h.. |