Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.53 - 45.81 MPa @Temperature -40.0 - 160 °C |
367 - 6644 psi @Temperature -40.0 - 320 °F |
Average value: 17.3 MPa Grade Count:1 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 2.53 - 45.81 MPa @Strain 1.68 - 146 % |
367 - 6644 psi @Strain 1.68 - 146 % |
Average value: 17.3 MPa Grade Count:1 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |