Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.250 - 2.50 MPa | 36.3 - 363 psi | |
MetaFoam Copper-Silver Foam General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional†metal foams. MetaFoam can .. |