Polymer Property : Tensile Strength, Ultimate = 3510 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate <= 24.2 MPa
<= 3510 psi
With carbon black or gum stocks. ASTM D412-80
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, General Description  (discontinu
Product form is white, odorless chips. Distinguishing Feature: Readily soluble in common solvents. Forms hard, glossy films.43 % Chlorine Content. 1.1% Sulfur Content. Very Good Abrasion Resista..