Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 337 MPa | 48900 psi | |
Pacific Sintered Materials FS-1602 Silicon Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 337 MPa | 48900 psi | |
PSM Industries Pacific Sintered Metals Silicon Iron FS-1602 Powdered Metal DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries |