Polymer Property : Tensile Strength, Ultimate = 3330 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3330 MPa
484000 psi
Toho Tenax Besfight® MC Type I (12,000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..
Tensile Strength, Ultimate 3330 MPa
484000 psi
Toho Tenax Besfight® MC Type I (3000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..
Tensile Strength, Ultimate 3330 MPa
484000 psi
Toho Tenax Besfight® MC Type I (6000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..